        H001: Polypropylene Homopolymer Flame Retardant

        Used in flame retardant of Polypropylene homopolymer and low ethylene content(≤8%) PP Copolymer.
        Online Inquiry
        Click Refresh Verification Code

        Product Details

        It can be widely used in flame retardant of Polypropylene homopolymer and low ethylene content(8%) PP Copolymer.

        With a low volume of addition(1-2%) and excellent performance of resisting plate-out, it is unnecessary to add antimonous

        oxide. The PP should be used to socket, Automobile  corrugated pipe, framework of electric appliance and shell of fan heater.


        I. Main Features

        1. Reaching UL94 V-2 of flame retardant rating with low volume of addition: 1.0-1.5% of Polypropylene homopolymer, 2.0-3.0%

        of low ethylene content PP Copolymer.

        2. Talcum powder, Barium sulfate and other inorganic filler(10-20%) are optional as additions.

        3. Antimonous oxide is unnecessary. No heavy metal.

        4. After baking for 300hoursat 70-80, the PP flame retardant produced with FR-NPB-H001, has excellent performance of resisting

        plate-out, mobility, light and heat.

        5. Meets the requirement of IEC60695-2-13 GWIT 775(3.0mm) and IEC60695-2-12 GWFI 960(3.0mm).

        6. The PP flame retardant produced with FR-NPB-C001 can meet the requirement of RoHS and REACH.


        II. Quality Index

        1. Appearance: Superfine white powder

        2. Loss on drying: 0.5%

        3. Decomposition temperature TGA2%):260


        . Toxicity

        1. LD50(Orally taken by Laboratory rat)>5300mg/kg(non-toxic)

        2. Potential carcinogenicityNO

        3. Skin irritationNO


        . Chief Application

        Sheet 1: System of No-filler PP flame retardant

        Test Item

        Test Standard

        Unit

        1

        2

        Polypropylene Homopolymer

        Low ethylene content   (8%) PP Copolymer

        1.0-2.0flame retardant

        2.0-3.0flame retardant

        Density

        ISO 1183

        g/cm3

        0.91

        0.91

        Melt Flow Index

        ISO 1133

        g/10min

        13.5

        12.1

        Tensile Strength

        ISO 527

        Mpa

        32

        26

        Elongation at Break

        ISO 527

        %

        50

        80

        Bending Modulus

        ISO 178

        Mpa

        1400

        1250

        Bending Strength

        ISO 178

        Mpa

        36

        32

        Notch Impact Strength

        ISO 180

        KJ/m2

        3.5

        8.0

        Flame Retardant Rating

        UL94

        3.20mm

        V-2

        V-2

        Flame Retardant Rating

        1.60mm

        V-2

        V-2


        Sheet 2: System of PP flame retardant filler

        Test Item

        Test Standard

        Unit

        1

        2

        PP+20%BaSO4

        PP+20%Talc

        2.0-3.0H001

        2.5-3.5H001

        Density

        ISO 1183

        g/cm3

        1.06

        1.06

        Melt Flow Index

        ISO 1133

        g/10min

        14.0

        13.0

        Tensile Strength

        ISO 527

        Mpa

        30

        30

        Elongation at Break

        ISO 527

        %

        30

        30

        Bending Modulus

        ISO 178

        Mpa

        1450

        1700

        Bending Strength

        ISO 178

        Mpa

        38

        40

        Notch Impact Strength

        ISO 180

        KJ/m2

        3.0

        3.0

        Flame Retardant Rating

        UL94

        3.20mm

        V-2

        V-2

        Flame Retardant Rating

        1.60mm

        V-2

        V-2

        Glowing Filament(GWIT)

        IEC 60695-2-13

        (2.0mm)

        775

        775

        Glowing Filament(GWIT)

        IEC 60695-2-12

        (2.0mm)

        960

        960


        . Notes

        1. Avoid Calcium Carbonate filler, which can interfere flame retarding feature.

        2. Accurate temperature control is required to avoid local overheating and causing volatilization in advance. Suggested

        processing temperature: 170-170-170-170-180-180-180- 180

        3. A little polypropylene powder is suggested as additive for uniform mixing and dispersing.

        4.Assembled screw elements should use weak shear to avoiding degrading of material.


        . Packaging

        Paper-poly or PP woven bag: 25kg/pack

        Remarks: low ethylene content(8%) Copolymer PP, such as: PP SP179, PP K9010 and PP AW19 etc.